Metal / Alloy |
Maximum operating temperature °C |
Melting Point °C
|
|
Copper |
150 |
1083 |
|
Brass |
N/A |
N/A |
|
Aluminium |
371 |
660 |
|
Monel |
538 |
1325 |
|
Mild Steel |
550 |
1525 |
|
Cupro Nickel 70/30 |
760 |
1230 |
|
Cast Iron |
870 |
1535 |
|
Stainless Steel AISI 304 |
900 |
1430 |
|
Stainless Steel AISI 316 |
900 |
1430 |
|
Stainless Steel AISI 310 |
1100 |
1400 |
|
Stainless Steel AISI 446 |
1150 |
1400 |
|
Inconel 600 |
1100 |
1400 |
|
Inconel 800 |
1100 |
1370 |
|
Hastelloy X |
1222 |
1300 |
|
Nicrobell B |
1250 |
1420 |
|
Nicrobell C |
1250 |
1420 |
|
Nickel |
1260 |
1455 |
|
Platinum |
1677 |
1773 |
|
Nibium |
1982 |
2497 |
|
Molybdenum |
2200 |
2620 |
|
Tantalum |
2480 |
2996 |
|